Small scale mechanical deformations have gained a significant interest over the past few decades, driven by the advances in integrated circuits and microelectromechanical systems. One of the most powerful and versatile characterization methods is the nanoindentation technique. The capabilities of these depth-sensing instruments have been improved considerably. They can perform experiments in vacuum and at high temperatures, such as in-situ SEM and TEM nanoindenters. This allows researchers to visualize mechanical deformations and dislocations motion in real time. Time-dependent behavior of soft materials has also been studied in recent research works. This Special Issue on "Small Scale Deformation using Advanced Nanoindentation Techniques"; will provide a forum for researchers from the academic and industrial communities to present advances in the field of small scale contact mechanics. Materials of interest include metals, glass, and ceramics. Manuscripts related to deformations of biomaterials and biological related specimens are also welcome. Topics of interest include, but are not limited to:

Small scale facture

Nanoscale plasticity and creep

Size-dependent deformation phenomena

Deformation of biological cells

Mechanical properties of cellular and sub-cellular components

Novel mechanical properties characterization techniques

New modeling methods

Environmentally controlled nanoindentation

In-situ SEM and TEM indentation

Médium Knihy     Paperback Book   (Kniha s mäkkou väzbou a lepeným chrbtom)
Vydané 11. júna 2019
ISBN13 9783038979661
Vydavatelia Mdpi AG
Strany 168
Rozmery 170 × 244 × 12 mm   ·   367 g
Jazyk Angličtina  

Viac od toho istého vydavateľa